Polymer Property : Drying Temperature = 203 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 95.0 °C
203 °F
Eastman EASTALLOY Polymer DA105, Natural Alloy  (discontinued **)
General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma..
Drying Temperature 95.0 - 150 °C
203 - 302 °F
Average value: 106 °C Grade Count:7
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Drying Temperature 95.0 - 110 °C

@Time <=7200 sec
203 - 230 °F

@Time <=2.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1700-7910 PPO, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Drying Temperature 95.0 - 110 °C

@Time <=7200 sec
203 - 230 °F

@Time <=2.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1700-8126 PPO, with glass spheres and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..
Drying Temperature 95.0 - 105 °C
203 - 221 °F
Injection Molding
LG Chemical LUPOY SC5004T PC/Polyester, Transparency
Description: Injection Molding, PC/Polyester, General Purpose, Transparency, High FlowApplication: Keypad for Mobile PhoneCAS: 103598-77-2Information provided by LG Chemical
Drying Temperature 95.0 - 110 °C
203 - 230 °F
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Drying Temperature 95.0 - 110 °C
203 - 230 °F
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Drying Temperature 95.0 - 110 °C

@Time <=7200 sec
203 - 230 °F

@Time <=2.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1700-7903 PPO, with glass fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..