Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 90.0 °C | 194 °F | |
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g.. |
|||
Drying Temperature | 90.0 °C | 194 °F | |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Drying Temperature | 90.0 °C @Time 7200 sec |
194 °F @Time 2.00 hour |
|
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Drying Temperature | 90.0 °C @Time 7200 sec |
194 °F @Time 2.00 hour |
|
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Drying Temperature | 90.0 °C | 194 °F | |
Pasargad Polymer Peyvand Pasamid 3P-H2000B Nylon 66 Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Drying Temperature | 90.0 - 110 °C @Time 14400 - 21600 sec |
194 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa PA6-MG45 45% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | Injection Molding |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | Injection Molding |
LG Chemical LUCEL N109LDS POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL N127-02 General Purpose POM, Unreinforced, Externally Lubricated, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | Injection Molding |
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
Drying Temperature | 90.0 °C | 194 °F | |
LG Chemical LUPOS GP-2106F General Purpose ABS, 10% Glass Fiber Reinforced, Weather Resistant, Flame Retardant LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 66 H2 G/50-GWHF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. improved G.W.F.I. compared to standard product.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 66 PA 66 Polyamide 66 (PA66). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latilub 66 Y/20 PA66, Aramid Fiber Reinforced Self-lubricating product based on Polyamide 66 (PA66). Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latilub 66-10T G/30-V0KB1 PA66, 10% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | |
LATI Latishield 66-10A PA66, Steel Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Drying Temperature | 90.0 °C | 194 °F | |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Drying Temperature | 90.0 °C | 194 °F | Extrusion |
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Pre-drying Temperature |
Asahi Kasei Xyron® 340W Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Pre-drying Temperature |
Asahi Kasei Xyron® 600H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latimass 62-05 D040 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |