Processing Properties Metric English Comments
Drying Temperature 60.0 - 80.0 °C

@Time 10800 - 14400 sec
140 - 176 °F

@Time 3.00 - 4.00 hour
Pre-drying; If stored for longer than 1 year
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PP HIP15025 HC Polypropylene
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH GF5030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPC B8075 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH B8065 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH GF35040 D PP, Glass Fiber-Reinforced, Chemically Coupled, Detergent Resistant
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Injection Molding
LG Chemical LUPOL HI5302RB PP+MF25%, High Impact
Description: Injection Molding, PP+MF25%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Extrusion Molding
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Injection Molding
LG Chemical LUPOL GP3400 PP+MF40%
Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Drying Temperature 60.0 - 80.0 °C
140 - 176 °F
Pre drying temp.
Supreme Petrochem SP 555 Flame Retardant Polystyrene
Characteristics Very good flow properties Good balance of toughness and rigidity Available in any dark colors Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxe..
Drying Temperature 60.0 - 80.0 °C
140 - 176 °F
( 2 hrs) Pre drying temp.
Supreme Petrochem SP 562 Flame Retardant Polystyrene
Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Low specific gravity Processing Injection moldingApplications Large size T.V. Cabinets Aud..
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Lubrizol Estane® S392A Thermoplastic Polyurethane
Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow ..
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Arkema Group Pebax® 7033 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Drying Temperature 60.0 - 80.0 °C
140 - 176 °F
( 2 hrs) Pre drying temp.
Supreme Petrochem SP 6630 Antistatic Polystyrene
Characteristics Easy flow Excellent transparency Processing Extrusion Applications For glossy cap layer on HIPS To prevent dust patterns on thermoformed products Material Status: Commercial : Acti..
Copyright © lookpolymers.com All Rights Reserved