Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Supreme Petrochem SP 6630 Antistatic Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Transparent Grade
Manufacturer Supreme Petrochem LTD
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Supreme Petrochem SP 6630 Antistatic Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics Easy flow Excellent transparency Processing Extrusion Applications For glossy cap layer on HIPS To prevent dust patterns on thermoformed products Material Status: Commercial : ActiveAgency Ratings: Information provided by Supreme Petrochem LTD
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 200 °C
15 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.6 MPa
6900 psi
50 mm/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
50 mm/min; ASTM D638
Flexural Strength 83.4 MPa

@Thickness 3.20 mm
12100 psi

@Thickness 0.126 in
ASTM D790
Flexural Modulus 2.84 GPa

@Thickness 3.20 mm
412 ksi

@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 0.200 J/cm

@Thickness 3.20 mm
0.375 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
ASTM D648
Vicat Softening Point 93.0 °C
199 °F
1kg / 120°C; ASTM D1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Surface Resistance 1.00e+11 - 1.00e+12 ohm
1.00e+11 - 1.00e+12 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature <= 230 °C
<= 446 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 60.0 - 80.0 °C
140 - 176 °F
( 2 hrs) Pre drying temp.