Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 143 - 149 °C | 290 - 300 °F | |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Drying Temperature | 143 - 149 °C | 290 - 300 °F | |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermotuf® OF-1006 HI Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades .. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Stat-Kon® LCL-4026 EM BK8-115 Polyetheretherketone, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(d Features: Electrically Conductive, Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discont.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® LF-1004 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Stat-Kon® EC-1004 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Stat-Kon® PDX-E-99550 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® EC-1006 EM Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® EF-1006 EM Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Drying Temperature | 130 - 149 °C | 266 - 300 °F | Average value: 138 °C Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Lubri-Tech™ SF-25GF/13T BLACK Polyphenylene Sulfide (PPS), Glass Filled, PTFE Lubricated
(discontinue Description/Features:Glass Fiber ReinforcedPTFE LubricatedBlackPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Edgetek® SF-35GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedUL 94 V0 (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Konduit® OTF-202-10 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically Conductive, Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; h.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Lubricomp® OCL-4534 EM Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant
(discont Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® OF-1008 Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® JF-1006 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Edgetek® PI-20CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Lubri-Tech™ PI-30GF/15T Polyetherimide (PEI), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Lubricomp® OCL-4536 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant
(discontinu Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Lubricomp® PDX-O-97635 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |