Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 85.0 °C @Time 14400 sec |
185 °F @Time 4.00 hour |
|
PlastiComp Complet® LGF30 - PA6 Nylon 6, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Drying Temperature | 85.0 °C @Time 14400 sec |
185 °F @Time 4.00 hour |
|
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 60% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Drying Temperature | 85.0 °C @Time 7200 - 14400 sec |
185 °F @Time 2.00 - 4.00 hour |
|
Polyplastic Armamid® PA 6-1FR Nylon 6, Flame Retardant Halogen and phosphor freeInformation provided by PolyPlastic Group. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 5202 HS BK-102 Nylon 66 (Dry)
(discontinued **) Capron 5202 HS BK-102 is an unfilled, heat stabilized, pigmented black nylon 6,6, injection molding compound. It combines strength and stiffness as well as excellent chemical resistance. The additi.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 5202 HS Blend Nylon 66 (Dry)
(discontinued **) Capron 5202 HS Blend is a blended, unfilled, heat stabilized, nylon 6,6, injection molding compound. It is also available in natural and pigmented versions. It combines strength and stiffness as wel.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 5202CQ Blend HS Blend Nylon 66 (Conditioned)
(discontinued **) Capron 5202CQ HS Blend is a heat stabilized, blended polyamide 6,6 injection molding homopolymer developed for fast molding cycles. It is also available in pigmented versions.Capron 5202CQ HS Blend.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8202 NL Nylon 6 (Dry)
(discontinued **) Capron 8202 NL is an unfilled, low viscosity, non-lubricated nylon 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is available in natural, heat sta.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8202C HS Nylon 6 (Conditioned)
(discontinued **) Capron 8202C HS is a heat stabilized, low viscosity, polyamide 6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It i.. |
|||
Drying Temperature | 85.0 °C @Time 14400 - 28800 sec |
185 °F @Time 4.00 - 8.00 hour |
|
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA) Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru.. |
|||
Drying Temperature | 85.0 °C | 185 °F | Injection |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | Injection |
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | Extrusion |
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | Extrusion |
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | Injection |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 1202CQ Nylon 6 (Conditioned)
(discontinued **) Capron 1202CQ is a blended low viscosity, polyamide 6 injection molding homopolymer, possessing a modified crystalline structure for increased property performance and faster cycles. It is also ava.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8232G HS BK-102 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G HS BK-102 is a pigmented black, heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8259 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8259 is a type 6 nylon injection molding graft copolymer developed for fastener applications requiring to abusive impact molding combined with a high level of pullout strength. It exhibits v.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8331G HS Blend Impact Modified, 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8331G HS Blend is a 14% glass fiber reinforced, heat stabilized, polyamide 6 molding compound developed for applications requiring improved toughness in combination with a balance of strength.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance .. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8362 HS Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS is a 34% glass reinforced, impact modified, heat stabilized nylon6 injection molding compound exhibiting a high level of toughness in combination with excellent processability and sur.. |
|||
Drying Temperature | 85.0 °C @Time 14400 sec |
185 °F @Time 4.00 hour |
|
PlastiComp Complet® LGF40 - PA66 Nylon 66, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Drying Temperature | 85.0 °C @Time 14400 sec |
185 °F @Time 4.00 hour |
|
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Drying Temperature | 85.0 °C | 185 °F | Injection |
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | Extrusion |
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,.. |