Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 453-45 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours if desired. |
ExxonMobil Santoprene® 8211-35W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours if desired. |
ExxonMobil Santoprene® 8211-45W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
ExxonMobil Santoprene® 151-60 Thermoplastic Rubber
(discontinued **) Description: A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
ExxonMobil Santoprene® 121-80M300 Thermoplastic Rubber
(discontinued **) Description: A black thermoplastic high-flow elastomer for excellent injection molding performance with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloropren.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
Advanced Elastomer Systems Santoprene® 8281-55 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant Dryer |
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Trefsin® 3101-75 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Trefsin® 3201-65 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | |
PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 82.0 - 104 °C | 180 - 219 °F | |
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether.. |
|||
Drying Temperature | 82.0 - 104 °C | 180 - 219 °F | |
DSM Biomedical PurSil® AL 20 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 10800 - 14400 sec |
180 - 199 °F @Time 3.00 - 4.00 hour |
|
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 sec |
180 - 199 °F @Time 2.00 hour |
|
Ineos ABS Lustran® 786 ABS, Extrusion Grade Lustran® ABS 786 resin is a black, virgin extrusion grade of ABS (acrylonitrile butadiene styrene). It is designed for extruded drain, waste, and vent (DWV) pipe. Lustran® ABS 786 (901046 blac.. |
|||
Drying Temperature | 82.0 - 85.0 °C | 180 - 185 °F | |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Drying Temperature | 82.0 - 85.0 °C | 180 - 185 °F | |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 82.0 °C | 180 °F | |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber
(discontinued **) A black thermoplastic general purpose elastomer designed for thin wall extrusion with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfo.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | |
PolyOne Edgetek® NL-45GF/000 Nylon 6/12 - 45% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 82.0 °C | 180 °F | |
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-80AEF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product l.. |