Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags.Features: Non-hygroscopic product, requires little to no drying before processingNeutral, easy coloring formulationUSP Class VI Certificate of ComplianceDrug Master File established with FDAProduct Notes: Values are for injection molded plaques, side gated.82.6 mm x 117.5 mm x 3 mmInformation provided by Advanced Elastomer Systems.Advanced Elastomer Systems is now a part of ExxonMobil. This grade was removed from the Advanced Elastomers Systems standard product line before the ExxonMobil acquisiton.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
5 seconds; ASTM D2240
95
95
5 seconds, After oven air aging 168 hours @ 150°C; ASTM D2240
Tensile Strength at Break 11.98 MPa
1737 psi
After oven air again 168 hrs. @ 150°C; ASTM D412
13.3 MPa
1930 psi
Across flow; ASTM D412
Tensile Strength, Yield 10.1 MPa
1460 psi
At 100% elongation, across flow; ASTM D412
Elongation at Break 315 %
315 %
After oven air aging 168 hrs. @ 150°C; ASTM D412
450 %
450 %
Across flow; ASTM D412
Tear Strength 75.4 kN/m
430 pli
73°F; ASTM D624
Compression Set 37 %
37 %
73°F, 170 hr, Method B; ASTM D395
Tensile Set 43 %
43 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -59.0 °C
-74.2 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 177 - 232 °C
351 - 450 °F
Drying Temperature 82.0 °C
180 °F
Desiccant Dryer
Dry Time 3 hour
3 hour
Desiccant Dryer
Copyright © lookpolymers.com All Rights Reserved