Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Kraton® G7820 GU-N (SEBS) Compound Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer A NSF certified, high hardness, multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by injectio.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3445DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4145 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4145 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4180 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4180 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4465 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4465 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3140 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3140 can be processed by injection molding or extrusion for appl.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Rear Barrel Temperature | 177 - 204 °C | 350 - 400 °F | Injection Molding |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Kraton® G7720 GI-N (SEBS) Compound Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |