Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products F22-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene, Black Applications: Support ductsHousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4802-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT5100-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G20P100-01UV 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Rigid exterior componentsHousingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC20P100-00 15% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC20P100-04 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, White Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC20P100-177UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, (Chrysler HS5) Gray Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products RCC120-01 20% Calcium Carbonate Reinforced Polypropylene, Black, Recycled Content Applications: Electrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products RCT120-01 20% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC and I/P ComponentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T10P100-01 10% Talc Reinforced Polypropylene, Black Applications: Consumer goodsAir ductsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P100-01EG 20% Talc Reinforced Polypropylene, General Purpose Black, Extrusion Grade Applications: Consumer goodsAutomotive componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T20P100-248 20% Talc Reinforced Polypropylene, General Purpose Grey Applications: Durable goodsElectronics housingsHVAC ducts - air distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP506-01 20% Talc Reinforced High Performance Polypropylene, Black Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Rear Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G20P100-406 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUEA) Midnight Black Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC20P600-01UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Sun roof trimFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP506-01B 22% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products M20P100-01A 20% Mica Reinforced Polypropylene, Black Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |