Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products FT3150-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsUnderhood componentsBumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Rear Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Rear Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Rear Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Rear Barrel Temperature | 221 - 271 °C | 430 - 520 °F | |
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Rear Barrel Temperature | 221 - 229 °C | 430 - 445 °F | |
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 221 - 229 °C | 430 - 445 °F | |
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 221 - 229 °C | 430 - 445 °F | |
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-IM1 Nylon 6, Impact Modified Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Rear Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Rear Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Rear Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
Rear Barrel Temperature | 221 °C | 430 °F | |
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa.. |
|||
Rear Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 221 - 271 °C | 430 - 520 °F | |
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced
(Unverified Da Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |