Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Rear Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 250°C |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Rear Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Injection Molding |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Rear Barrel Temperature | 230 - 235 °C | 446 - 455 °F | Injection Molding |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Rear Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical Lupox® HI-2302 High Impact PBT, 30% Glass Fiber Reinforced LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Rear Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical Lupox® PBT-GP-2306F 30% GFR Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 230 - 270 °C | 446 - 518 °F | |
LG Chemical LUPOY GP-5000FQ General Purpose PC/ABS Alloy, Unreinforced, Excellent Flow Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Rear Barrel Temperature | 230 - 270 °C | 446 - 518 °F | |
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Rear Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 250°C |
Kingfa LONOY 2100 LT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Start Point: 240°C |
Kingfa MAC-551 PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Rear Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical Lupox® SG-4405 Surface Gloss PBT, 40% Glass Fiber/Mineral Reinforced, Dimensional Stability LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Rear Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samyang Triloy® 120H PC/ABS alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Rear Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samyang Triloy® 170 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Rear Barrel Temperature | 230 - 280 °C | 446 - 536 °F | |
Teknor Apex Beetle® 60GS6 Nylon 6, 30% Glass Bead Reinforced, Dry Features: High rigidity and low warping. Processing Method: Injection MoldingForms: Pellets Injection Notes: Drying is necessary if material has been exposed to air for longer than 3 hours; Back Pr.. |
|||
Rear Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Unitika UM-8430RG Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 1 |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 1 |
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Beijing Chemical Industry KAIFA® MN201-G25 Nylon 66 Resin 25% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Beijing Chemical Industry KAIFA® MN301-G20 Nylon 66 Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Beijing Chemical Industry KAIFA® MN301-G35 Nylon 66 Resin 35% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samyang Triloy® 210N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantHeat resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |