Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 150 - 175 °C | 302 - 347 °F | |
Resinoid 2002-4 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 150 - 175 °C | 302 - 347 °F | |
Resinoid 2002-C5 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 80.0 - 175 °C | 176 - 347 °F | Average value: 121 °C Grade Count:5 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Mold Temperature | 80.0 - 175 °C | 176 - 347 °F | Average value: 112 °C Grade Count:10 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Mold Temperature | 150 - 175 °C | 302 - 347 °F | |
Resinoid 2016 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 150 - 175 °C | 302 - 347 °F | |
Resinoid 2016P Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 150 - 175 °C | 302 - 347 °F | |
Resinoid 2018 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |