Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 140 - 160 °C | 284 - 320 °F | DAM |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Lehmann & Voss LUVOCOM® 20-0778/BK Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Lehmann & Voss LUVOCOM® 20-7314 Polyphthalamide, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Lehmann & Voss LUVOCOM® 20-7324 Polyphthalamide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Lehmann & Voss LUVOCOM® 20-7343 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Lehmann & Voss LUVOCOM® 20-7970 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Lehmann & Voss LUVOCOM® 20-8112 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Lehmann & Voss LUVOCOM® 20-8283 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Lehmann & Voss LUVOCOM® 20-8302 Polyphthalamide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Mold Temperature | 120 - 160 °C | 248 - 320 °F | |
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Solvay Specialty Polymers PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-351 resin is a higher flow, injection molding grade of PrimoSpire® self-reinforced polyphenylene (SRP). PrimoSpire® SRP resin is an ultra-high performance amorphous, melt-pro.. |
|||
Mold Temperature | 130 - 160 °C | 266 - 320 °F | |
Covestro Apec® DP1-9389/5 Polycarbonate Developmental producteasy flowingeasy to demoldsoftening temperature (VST/B 120)=218 °CPreprocessingMax. Water content |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
E-Polymers SEPAZ® V200L Unfilled PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
E-Polymers SEPAZ® V230B 30% Mineral Filled Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Mold Temperature | 130 - 160 °C | 266 - 320 °F | |
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Mold Temperature | 149 - 160 °C | 300 - 320 °F | |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Product Introduction: Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC t.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Mold Temperature | 135 - 160 °C | 275 - 320 °F | |
E-Polymers SEPAZ® V330FR 30% Glass Fiber Reinforced Flame Retardant PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Mold Temperature | 120 - 160 °C | 248 - 320 °F | |
BASF Ultrason S 6010 PSU Ultrason S 6010 is an unreinforced, high molecular weight injection-molding and extrusion grade with excellent chemical resistance (stress crack resistance) and good solubility in typical solvents (.. |
|||
Mold Temperature | 130 - 160 °C | 266 - 320 °F | |
E-Polymers SEPAZ® K130IM 30% Glass Fiber Reinforced Impact Modified PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |