Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT5100-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products GC30P104-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 32.2 - 48.9 °C | 90.0 - 120 °F | |
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor.. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products HP531-678UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, IT3A Medium Light Stone Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP 1166B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP 1225 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1274G Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2150 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2156 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1353A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1852A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2770L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer.. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products CC20P200-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products GC20P100-01 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |