Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 161J-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 161J-4-DD Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 161JA White Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging 4195 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 01FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 13FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging PK8-1080 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging VB9-51 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 207 °C | 390 - 405 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging XPL 355GC Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 207 °C | 390 - 405 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging XPL189 Amber 1505 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI) Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI) Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI) Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI) Torlon® 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a .. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI) Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI) Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI) Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |
|||
Mold Temperature | 199 - 216 °C | 390 - 421 °F | |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |