Material Notes:
The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Density 0.785 g/cc
0.0284 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Hardness, Shore D 78
78
15 sec; ASTM D2240
82
82
ASTM D2240
Tensile Strength, Yield 43.4 MPa
6290 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.66 GPa
386 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 79.3 MPa
11500 psi
ASTM D790
Flexural Modulus 2.96 GPa
429 ksi
ASTM D790
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C

@Thickness 3.18 mm
151 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Vicat Softening Point 81.0 °C
178 °F
Processing Properties Metric English Comments
Mold Temperature 199 - 213 °C
390 - 415 °F
Blow Molding
Descriptive Properties Value Comments
Features General Purpose
High Gloss
High Impact Resistance
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose
Packaging
Sheet
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved