Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 166 °C | 150 - 331 °F | |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Mold Temperature | 65.6 - 166 °C | 150 - 331 °F | |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1603 Multi-purpose grade BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1902 Mineral Filled Alkyd BMC 1902 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression molding. It was developed primarily for applications requiring very good impact and flex.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 3001H Mineral Filled Alkyd BMC 3001H molding compound is a mineral filled, glass-fiber reinforced alkyd compound suitable for compression and transfer molding. Because of its soft flow, it is also used extensively in cold spu.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical app.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 605LWR Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LWR is a mineral filled, glass fiber reinforced polyester bulk molding compound suitable for compression, transfer and stuffer injection molding. It is designed to provide improved wear resis.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound BMC 610 molding compound is a mineral filled, glass fiber reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC SLC 1000 Glass Reinforced Polyester BMC SLC 1000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. It is V-0 flame arc and track resistant. UL® recognized. This material was formerly known.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1412 Flame and Track Resistant BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1423 Wear Resistant, Electrical Grade BMC 1423 is a wear-resistant electrical grade material used in applications where there are moving parts. Best anti-wear properties are exhibited when used in conjunction with mating parts molded fr.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 810 General Purpose Molding Compound BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Mold Temperature | 65.6 - 166 °C | 150 - 331 °F | |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |