Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 140 - 155 °C | 284 - 311 °F | for optimal gloss and heat resistance |
Idemitsu Kosan Xarec® EA 528 SPS, 30% Glass Filled
(discontinued **) Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ CLS 5000 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ FFSL 7061 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ FSL 7641 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ FSL 7651 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LIM 6040 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LIM 9071E Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2040 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2530 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2620 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 LV Liquid Silicone Rubber - Low Volatile / High Tear This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2742 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3696/20 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4030 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4660 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 7080 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4080 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 7060 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | |
Eurotec® Tecomid® NT40 GR60 NL HS PPA, 60% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 140 °C | 284 °F | |
Bulk Molding Compounds BMC 665 Mineral filled, 20% glass reinforced polyester molding compound Description: BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good.. |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | Injection molding |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | Injection molding |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Silopren™ LSR 3386/30 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Silopren™ LSR 4060 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |