Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Oxford Polymers C-Acetal 10MF-900 BK Acetal Product Description: Acetal Injection Molding Grade, 10 melt flow Processing and Delivery Form: Pellets and Injection MoldingSpecial Characteristics: Pre-colored blackInformation provided by Oxford.. |
|||
Nozzle Temperature | 182 - 204 °C | 360 - 400 °F | |
Fiberfil® M-1492 BK223 Polypropylene Homopolymer, Glass Reinforced, mica Filled, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 204 °C | 360 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and .. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2840 Thermoplastic Elastomer Elastocon® 2840 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2840 is FDA compliant and well suited for cons.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2870 Thermoplastic Elastomer Elastocon® 2870 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2870 is FDA compliant and well suited for cons.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2880L Thermoplastic Elastomer Elastocon® 2880L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2880L is FDA compliant and well s.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2890 Thermoplastic Elastomer Elastocon® 2890 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2890 is FDA compliant and well suited for cons.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited.. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8048N Thermoplastic Elastomer Elastocon® 8048N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8048N is FDA compliant and well suited.. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui.. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8058HL Thermoplastic Elastomer Elastocon® 8058HL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058HL is FDA compliant a.. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8058N Thermoplastic Elastomer Elastocon® 8058N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8058N is FDA compliant and well suited.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8078B Thermoplastic Elastomer Elastocon® 8078B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078B is well suited for consumer goods a.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8078N Thermoplastic Elastomer Elastocon® 8078N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078N is FDA compliant and well suited.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer Elastocon® 8078NL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a scratch and mar resistant surface finish. Elastocon® 8078NL is FDA c.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer Elastocon® 8088BL is a black lubricated thermoplastic elastomer formulated for applications that require high impact resistance and a reduced coefficient of friction. Elastocon® 8088BL is well sui.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8088N Thermoplastic Elastomer Elastocon® 8088N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8088N is FDA compliant and well suited.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer.. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8150B Thermoplastic Elastomer Elastocon® 8150B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8150B is well suited for consumer goods a.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer Elastocon® CLR40 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR40 is.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® CLR45 Thermoplastic Elastomer Elastocon® CLR45 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR45 is.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® CLR65 Thermoplastic Elastomer Elastocon® CLR65 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a tactile surface finish. Elastoc.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® CLR75 Thermoplastic Elastomer Elastocon® CLR75 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface fin.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® OF65 Thermoplastic Elastomer Elastocon® OF65 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a reduced coefficient of f.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela.. |