Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 170 - 190 °C | 338 - 374 °F | |
Multibase TPSiV® 4000-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 98 AE Thermoplastic Polyurethane Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Nozzle Temperature | 170 - 190 °C | 338 - 374 °F | |
Huntsman AVALON® 65 AC Thermoplastic Polyurethane Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 65 AE Thermoplastic Polyurethane Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport.. |
|||
Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
Huntsman AVALON® 70 AE Thermoplastic Polyurethane Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 85 AE Thermoplastic Polyurethane Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 92 AE Thermoplastic Polyurethane Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 95 AE Thermoplastic Polyurethane Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | Extrusion |
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext.. |
|||
Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
Lubrizol Estane® T365A Thermoplastic Polyurethane Type: Estane® T365A is a Shore 70A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
Lubrizol Estane® T465A Thermoplastic Polyurethane Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | Injection |
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |