Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical HI100H ABS, High Impact, High Toughness Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP2200 PP+GF20% Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HI5204H PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HF5150H PP+MF15%, High Flow Description: Injection Molding, PP+MF15%, High FlowApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HM3102A PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HM3207 PP+MF20%, High Stiffness Description: Injection Molding, PP+MF20%, Good Weatherability, High StiffnessApplication: Automotive Interior Parts CAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HM5204 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5007B PP+Rubber, High Impact Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem AB870LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem DIOSHY® GP-935-UB2 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem GP-975 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem HP-930NC-HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem LP-855 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem 475-845N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 190 - 230 °C | 374 - 446 °F | |
Teknor Apex Uniprene® 7010-64NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Nozzle Temperature | 190 - 230 °C | 374 - 446 °F | |
Teknor Apex Uniprene® UN-2023 Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Nozzle Temperature | 190 - 230 °C | 374 - 446 °F | |
Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Nozzle Temperature | 190 - 230 °C | 374 - 446 °F | |
Teknor Apex Uniprene® UN-7010-40D-NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Nozzle Temperature | 190 - 230 °C | 374 - 446 °F | |
Teknor Apex Uniprene® UN-7100-73 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection |
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |