Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 166 - 204 °C | 331 - 399 °F | |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Oxford Polymers C-Acetal 10MF-900 BK Acetal Product Description: Acetal Injection Molding Grade, 10 melt flow Processing and Delivery Form: Pellets and Injection MoldingSpecial Characteristics: Pre-colored blackInformation provided by Oxford.. |
|||
Nozzle Temperature | 177 - 204 °C | 351 - 399 °F | |
PolyOne Dynaflex™ D3202-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3202-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -.. |
|||
Nozzle Temperature | 166 - 204 °C | 331 - 399 °F | |
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - .. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 399 °F | |
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 399 °F | |
PolyOne Dynaflex™ G7930-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 399 °F | |
PolyOne Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Nozzle Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Nozzle Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Nozzle Temperature | 182 - 204 °C | 360 - 400 °F | |
Fiberfil® M-1492 BK223 Polypropylene Homopolymer, Glass Reinforced, mica Filled, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 204 °C | 360 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and .. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2840 Thermoplastic Elastomer Elastocon® 2840 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2840 is FDA compliant and well suited for cons.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2870 Thermoplastic Elastomer Elastocon® 2870 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2870 is FDA compliant and well suited for cons.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2880L Thermoplastic Elastomer Elastocon® 2880L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2880L is FDA compliant and well s.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2890 Thermoplastic Elastomer Elastocon® 2890 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2890 is FDA compliant and well suited for cons.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited.. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8048N Thermoplastic Elastomer Elastocon® 8048N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8048N is FDA compliant and well suited.. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8058N Thermoplastic Elastomer Elastocon® 8058N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8058N is FDA compliant and well suited.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8078B Thermoplastic Elastomer Elastocon® 8078B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078B is well suited for consumer goods a.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer Elastocon® 8078NL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a scratch and mar resistant surface finish. Elastocon® 8078NL is FDA c.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer Elastocon® 8088BL is a black lubricated thermoplastic elastomer formulated for applications that require high impact resistance and a reduced coefficient of friction. Elastocon® 8088BL is well sui.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8088N Thermoplastic Elastomer Elastocon® 8088N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8088N is FDA compliant and well suited.. |
|||
Nozzle Temperature | 188 - 204 °C | 370 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer.. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8150B Thermoplastic Elastomer Elastocon® 8150B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8150B is well suited for consumer goods a.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® CLR65 Thermoplastic Elastomer Elastocon® CLR65 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a tactile surface finish. Elastoc.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® CLR75 Thermoplastic Elastomer Elastocon® CLR75 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface fin.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela.. |