Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 246 - 279 °C | 475 - 535 °F | |
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 246 - 279 °C | 475 - 535 °F | |
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Beetle® 102 Nylon 66, Unreinforced, Nucleated Notes: Nucleated for fast cycling; Improved strength and rigidity; FMVSS Flammability: Passes, FMVSS 302Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Front Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Beetle® 140 BH Nylon 66, Glass Bead Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Front Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced Notes: MoS2 modified; Molybdenum disulphide modified to provide self-lubrication and low friction to parts subjected to wear and abrasion. FMVSS Flammability: Passes, FMVSS 302Processing Method: Inj.. |
|||
Front Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Front Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Chemlon® 113 GH Nylon 66, 13% Short Glass Fiber Reinforced Features: Good creep Resistance; Good stiffness; Good dimensional stability; High strength; Heat stabilized Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS.. |
|||
Front Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Chemlon® 143 G Nylon 66, 43% Short Glass Fiber Reinforced Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |