Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 229 - 252 °C
445 - 485 °F
Teknor Apex Chemlon® 253 Nylon 6, Toughened
Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation ..
Middle Barrel Temperature 229 - 252 °C
445 - 485 °F
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified
Notes: Very high impact and elongation, low flexural modulus material for tubing and wire jacketing applications requiring a soft, flexible product; FMVSS Flammability: Passes, FMVSS 302Processing M..
Middle Barrel Temperature 229 - 252 °C
445 - 485 °F
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced
Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex..
Middle Barrel Temperature 229 - 252 °C
445 - 485 °F
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor..