Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Middle Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources PC/TP-GP3 PC/Polyester Alloy High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Middle Barrel Temperature | 232 - 277 °C | 450 - 530 °F | |
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA S610 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA T-120 Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA TW-23V Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA/PC TA-35 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 277 °C | 450 - 530 °F | |
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced
(Unverified Da Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |