Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
Multibase Multi-Pro® 2514 XU Polypropylene Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase |
|||
Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P104-00 Polypropylene, Natural Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P107-00 Polypropylene Homopolymer, Natural Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P250-01 Polypropylene Copolymer, Black Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P256-00 Polypropylene Copolymer, Natural Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P601-01 Polypropylene Copolymer, Black Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 379 - 430 °F | |
PolyOne Versaflex™ CL2242 Thermoplastic Elastomer (TPE) Versaflex™ CL2242 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP... |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 2040 Polypropylene Copolymer X-PRO PP 2040 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 3020 Polypropylene Copolymer X-PRO PP 3020 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 5002 Polypropylene Copolymer X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
LTL Color Compounds ColorFast® FRPS100 Styrene, High Impact V1-rated high impact styreneAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
LTL Color Compounds ColorFast® FRPS200 Styrene, High Impact V0/5VA high impact styreneAll information provided by LTL Color Compounders, Inc. |