Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
50%; Recommended for 1/8" dia bead |
Parker Chomerics Tecknit® 72-00152 Silver-Filled Flexible Resin Caulking System Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide .. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
|
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Cure Time | 4320 - 7200 min @Temperature 25.0 °C |
72.0 - 120 hour @Temperature 77.0 °F |
Complete Cure Cycle |
Northstar Polymers MCP-V40A Polyurethane Gel MCP-V40A is a polyurethane gel formulation specifically designed for padding and cushioning applications, where low rebound property of the material is critical. This viscoelastic polymer is a two.. |
|||
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
50%; Recommended for 1/8" dia bead |
Parker Chomerics Tecknit TeckBond™-C Silver-Plated Copper-Filled Adhesive Description: TECKBOND-C is a silicone rubber base filled with silver-plated copper particles to produce a highly conductive one-component adhesive sealant. The system is an RTV moisture-cured compou.. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
Zinc, full strength |
Permabond HM163 Anaerobic Retainer Permabond® HM163 is a medium viscosity, thixotropic anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It has been specifically formulated to provide a .. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
M10 steel, full strength |
Permabond LM113 Anaerobic Threadlocker Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop.. |
|||
Cure Time | 4320 - 5760 min @Temperature 25.0 °C |
72.0 - 96.0 hour @Temperature 77.0 °F |
Full |
Lord Adhesives Thermosetâ„¢ UR-329 Two Component Urethane Potting Compound Lord UR-329 is a flexible, two-component, room temperature curing, urethane, encapsulating compound. UR-329 maintains low hardness and modulus over a wide temperature range, which imparts minimal st.. |
|||
Cure Time | 4320 - 18000 min @Temperature 23.9 °C |
72.0 - 300 hour @Temperature 75.0 °F |
|
Master Bond EP21LVSP6 Two component epoxy for bonding, sealing, coating and encapsulating Product Description: Master Bond EP21LVSP6 is a two component epoxy compound for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at room temperature or more ra.. |
|||
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
|
Tra-Con Tra-Bond 724-14C Polyurethane Adhesive TRA-BOND 724-14C premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar.. |
|||
Cure Time | 4320 min @Temperature 10.0 °C |
72.0 hour @Temperature 50.0 °F |
Full Load |
Chesterton ARC 791 Composite Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex.. |
|||
Cure Time | 4320 min @Temperature 10.0 °C |
72.0 hour @Temperature 50.0 °F |
Full Load |
Chesterton ARC 982 100% Novolac acid resistant coating Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo.. |
|||
Cure Time | 4320 min @Temperature 16.0 °C |
72.0 hour @Temperature 60.8 °F |
Overcoat End |
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b.. |
|||
Cure Time | 4320 min @Temperature 32.0 °C |
72.0 hour @Temperature 89.6 °F |
Full Mechanical/Chemical |
Chesterton ARC MXHT High temperature severe wear compound Description: An advanced ceramic composite for the protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack at elevated temperatures. It is applied at a thickness o.. |
|||
Cure Time | 4320 min @Temperature 10.0 °C |
72.0 hour @Temperature 50.0 °F |
Full Load |
Chesterton ARC PW Potable Water Coating Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total.. |
|||
Cure Time | 4320 min @Temperature 10.0 °C |
72.0 hour @Temperature 50.0 °F |
Full Chemical |
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be pres.. |
|||
Cure Time | 4320 - 7200 min @Temperature 25.0 °C |
72.0 - 120 hour @Temperature 77.0 °F |
|
Cytec Conathane® CE-1175 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
|
Epoxy Technology EPO-TEK® EJ2189-LV Electrically Conductive Epoxy Low Viscosity, two component room temp curing conductive epoxyInformation Provided by Epoxy Technology |
|||
Cure Time | 4320 min @Temperature 32.0 °C |
72.0 hour @Temperature 89.6 °F |
Full Mechanical |
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with .. |
|||
Cure Time | 4320 min @Temperature 10.0 °C |
72.0 hour @Temperature 50.0 °F |
Full Load |
Chesterton ARC MX2 High Wear Fine Particle Wear Compound Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”.. |
|||
Cure Time | 4320 min @Temperature 16.0 °C |
72.0 hour @Temperature 60.8 °F |
Full Chemical |
Chesterton ARC MX2 High Wear Fine Particle Wear Compound Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”.. |
|||
Cure Time | 4320 - 7200 min @Temperature 24.0 °C |
72.0 - 120 hour @Temperature 75.2 °F |
full cure |
BCC Products BC 8990 Polyurethane Elastomer BC8990 is a two-component urethane elastomer compound specifically designed for general purpose molding and casting of various shapes. This product is a safe, easy-to-handle, room temperature mixing.. |
|||
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
|
Atom Adhesives AA-BOND FDA16 Epoxy Adhesive AA-BOND FDA16 is a medium viscosity epoxy resin system specifically developed for medical device applications. AA-BOND FDA16 has been tested in accordance with USP biological reactivity tests, in vi.. |
|||
Cure Time | 4320 - 7200 min @Temperature 24.0 °C |
72.0 - 120 hour @Temperature 75.2 °F |
full cure |
BCC Products BC 8675E Polyurethane Elastomer BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f.. |
|||
Cure Time | 4320 min @Temperature 16.0 °C |
72.0 hour @Temperature 60.8 °F |
Full Chemical |
Chesterton MRS 58 Metal Rebuilding System An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 1.5 mm (60 mils) or mo.. |