Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 30.0 °C
0.0500 hour

@Temperature 86.0 °F
85% RH
Parker Chomerics CHO-FORM 5532 EMI Shielding Material
One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 553..
Cure Time 3.00 min

@Temperature 150 °C
0.0500 hour

@Temperature 302 °F
Parker Chomerics THERM-A-FORM T642 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Cure Time 3.00 min

@Temperature 150 °C
0.0500 hour

@Temperature 302 °F
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Cure Time 3.00 min

@Temperature 150 °C
0.0500 hour

@Temperature 302 °F
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Cure Time 3.00 min

@Temperature 260 °C
0.0500 hour

@Temperature 500 °F
Wave Solder
Parker Chomerics CHO-FLEX 601 Conductive Coating
CHO-FLEX™ 601 coating is specifically designed for EMI shielding of copper/Kapton flexible circuit laminates and for printing circuits on Kapton film. Upon cure, this coating exhibits excellent adh..
Cure Time 3.00 min

@Temperature 155 °C
0.0500 hour

@Temperature 311 °F
ts2
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 3.00 min

@Temperature 150 °C
0.0500 hour

@Temperature 302 °F
Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System
Cure 6 minutes at 130°C or 3 minutes at 150°C.TIGA 905 is a stress-absorbing and electrically conductive, silver-filled epoxy adhesive recommended for solder replacement in microelectronic interco..
Cure Time 3.00 min

@Temperature 120 °C
0.0500 hour

@Temperature 248 °F
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive
CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o..
Cure Time 3.00 min

@Temperature 204 °C
0.0500 hour

@Temperature 399 °F
Lord Adhesives Flocklok® 852 Flock Adhesive
LORD Flocklok® 852 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good res..
Cure Time 3.00 min

@Temperature 204 °C
0.0500 hour

@Temperature 399 °F
Lord Adhesives Flocklok® 853 Blocked Flock Adhesive
Flocklok® 853 is a blocked, heat-curing, single coat adhesive used to adhere polyester or nylon fibers (flock) to a variety of elastomers including EPDM, NR, CR, and SBR. Flocked substrates provi..
Cure Time 3.00 min

@Temperature 204 °C
0.0500 hour

@Temperature 399 °F
Lord Adhesives Flocklok® 853A Flock Adhesive
LORD Flocklok® 853A is a blocked, heat-curing, singlecoat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates pro..
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
Gwent Electronic Materials C2050712D58 Silver Ink for ITO Substrates
This product is based on a unique curing process that results in the low temperature formation of a thermosetting polymer. Inks containing these polymers combine excellent chemical, environmental a..
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
Gwent Electronic Materials C2070126D4 High Brightness Phosphor Ink (Orange)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
Gwent Electronic Materials C2070126P5 High Brightness Phosphor Ink (White)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
Gwent Electronic Materials C2090819P2 Silver Ink
This product is part of a range of Heat Curable Inks designed specifically for use in Photovoltaic panels. These products are based on a unique curing process that results in the low temperature fo..
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
Gwent Electronic Materials C2101125P4 High Brightness Phosphor Ink
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
Cure Time 3.00 min

@Temperature 95.0 °C
0.0500 hour

@Temperature 203 °F
Tra-Con Tra-Bond 224-1 Rapid Room Temperature Cure Epoxy Adhesive
TRA-BOND 224-1 room temperature curing epoxy adhesive develops structural strength rapidly. Unlike most "rapid cure" epoxies which gel in one or two minutes, TRA-BOND 224-1 adhesive exhibits a 30 mi..
Cure Time 3.00 min

@Temperature 150 °C
0.0500 hour

@Temperature 302 °F
Tra-Con Tra-Bond 77-1S One Component SMD Adhesive
TRA-BOND 77-1S one component, solvent-free, insulating epoxy adhesive is designed specifically for attaching surface mounted devices (SMDs) to printed circuit boards prior to wave solder. TRA-BOND 7..
Cure Time 3.00 min

@Temperature 100 °C
0.0500 hour

@Temperature 212 °F
Dow Corning 3-4207 DIELECTRIC TOUGH GEL KIT
Two-part, translucent green, fast RT or heat cure, tough, primerless chemical adhesion, UV indicator, and UL 94 V-1 flammability classification.Information provided by Dow Corning
Cure Time 3.00 min

@Temperature 232 °C
0.0500 hour

@Temperature 450 °F
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 5388 is a one-part, blue pigmented, rapid heat curing powder resin, designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a var..
Cure Time 3.00 - 4.98 min

@Temperature 75.0 °C
0.0500 - 0.0830 hour

@Temperature 167 °F
Recoat, at 50% humidity
Blue River Coatings Acrylic 4000D Topcoat
BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo..
Cure Time 3.00 min

@Temperature 140 °C
0.0500 hour

@Temperature 284 °F
Dry to stack, at 50% humidity
Blue River Coatings Semi-Transparent Wood Stain Concentrate
BLUE RIVER COATINGS Semi-Transparent Wood Stain is a water based stain developed to provide long lasting protection and a beautiful appearance on wood surfaces. BLUE RIVER COATINGS Semi-Transparent ..
Cure Time 3.00 min

@Temperature 155 °C
0.0500 hour

@Temperature 311 °F
ts2
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
Gwent Electronic Materials C2090210P12 Silver Ink
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
Gwent Electronic Materials R2070613P2 Resin Binder
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. Phosphor Inks containing these polymers combine excellent chemical, environmental w..
Cure Time 3.00 - 4.98 min

@Temperature 75.0 °C
0.0500 - 0.0830 hour

@Temperature 167 °F
Recoat, at 50% humidity
Blue River Coatings Acrylic 4000 Topcoat
BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo..