Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 185 - 210 °C | 365 - 410 °F | |
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE) OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af.. |
|||
Zone 4 | 185 - 199 °C | 365 - 390 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolys.. |
|||
Zone 4 | 185 - 205 °C | 365 - 401 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1030D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 4 | 185 - 200 °C | 365 - 392 °F | Extrusion Molding |
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon. |
|||
Zone 4 | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound |
|||
Zone 4 | 185 - 200 °C | 365 - 392 °F | Extrusion Molding |
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 4 | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane ApplicationsInjectionIndustry Parts Information provided by API-Kolon. |
|||
Zone 4 | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-590A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Zone 4 | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Zone 4 | 185 - 195 °C | 365 - 383 °F | Extrusion Molding |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 4 | 185 - 215 °C | 365 - 419 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Zone 4 | 185 - 193 °C | 365 - 380 °F | |
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Zone 4 | 185 °C | 365 °F | |
SK Chemicals SKYTHANE® CR180A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 4 | 185 °C | 365 °F | |
Borealis Visico™/Visico™ ME4425/LE4438 Polyethylene Visico™ ME4425 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ ME4425 and Visico™ LE4438 is a combination of a Visico™ bas.. |
|||
Zone 4 | 185 - 195 °C | 365 - 383 °F | Injection |
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 4 | 185 - 195 °C | 365 - 383 °F | Injection |
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 4 | 185 °C | 365 °F | Blown Film Coextrusion |
DuPont™ Appeel® 72D799 Sealing Resin DuPont™ Appeel® 72D799 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP.. |
|||
Zone 4 | 185 °C | 365 °F | Blown Film Coextrusion |
DuPont™ Appeel® 72D811 Sealing Resin DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion.. |
|||
Zone 4 | 185 °C | 365 °F | Blown Film Coextrusion |
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Zone 4 | 185 °C | 365 °F | Blown Film Coextrusion |
DuPont™ Bynel® 41E755 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Zone 4 | 185 °C | 365 °F | Blown Film Extrusion |
DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate Elvaloy® AC 1330 is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A.. |
|||
Zone 4 | 185 °C | 365 °F | Blown Film Coextrusion |
DuPont™ Elvax® 3128-1 Ethylene Vinyl Acetate DuPont™ Elvax® 3128-1 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® .. |
|||
Zone 4 | 185 °C | 365 °F | Blown Film Coextrusion |
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle.. |
|||
Zone 4 | 185 °C | 365 °F | |
Equate EFDC-7087 LLDPE Film Extrusion Resin EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-.. |
|||
Zone 4 | 185 °C | 365 °F | Blown Film Coextrusion |
DuPont™ Surlyn® 1707 Sodium Ionomer Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Zone 4 | 185 °C | 365 °F | Blown Film Coextrusion |
DuPont™ Surlyn® 1825 Zinc Ionomer Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp.. |
|||
Zone 4 | 185 °C | 365 °F | Extrusion |
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 80AT3 NAT 022 is an 80A non halogen, flame retardant, aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Transparent spherical pelletsFeatures: Zero halogenUses.. |