Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7916 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7938/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7995 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8099 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8102 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8161 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8167 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8179 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8199 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8264 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8320 PEEK, with aramid reinforcement and PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/GF/30/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/RD7405 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/XCF/20 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-0699-1 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-0856/GY7 PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7023/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7596/BL PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7731/BL PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8402 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7918 PEEK, unreinforced Applications: medical engineeringEspecially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical resistance parts, non flammable.Inherent flame resistance.S.. |