Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 155 - 170 °C | 311 - 338 °F | Extrusion Molding |
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon. |
|||
Zone 1 | 155 - 170 °C | 311 - 338 °F | Extrusion Molding |
Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionCompoundingIndustry PartsParts for Automobile/Mobile phoneAcetal Compound Information provided by API-Kolon. |
|||
Zone 1 | 155 - 170 °C | 311 - 338 °F | Injection Molding |
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 155 - 170 °C | 311 - 338 °F | Extrusion Molding |
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 150 - 170 °C | 302 - 338 °F | Injection Molding |
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon. |
|||
Zone 1 | 150 - 170 °C | 302 - 338 °F | Injection Molding |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEMâ€; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |