Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-1114 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7532 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.dynamic st.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-8520 Polyamide 66, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® NSB 90 NT Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1/AR/5/NT Polyamide 66, with aramid reinforcement Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Isotropic shrinkage characteristics.Control disks, cams, s.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-0784 Polyamide 66, with glass fiber and carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-0867 Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-1119 VP Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7139-1 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® G Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss PLASLUBE NY-1/TF/20/BK Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 290 °C | 554 °F | Feed zone |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Zone 1 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7003 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |