Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Die Temperature = 419 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 215 °C
419 °F
Zone 3
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
Die Temperature 215 - 255 °C
419 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1063D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 215 - 255 °C
419 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1163D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 215 - 255 °C
419 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3047D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 215 - 220 °C
419 - 428 °F
Lubrizol Advanced Materials PEARLTHANE® 11T98 Thermoplastic Polyurethane Elastomer
PEARLTHANE® 11T98 is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, combining high hardness with excellent mechanical properties. It can be extruded..
Die Temperature 215 °C
419 °F
Taiwan PU Corporation TPU-E98 General Grade, Extrusion Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation.
Die Temperature 215 °C
419 °F
Taiwan PU Corporation TPUI-ED64 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Die Temperature 215 - 230 °C
419 - 446 °F
Solvay TECHNYL® C 536XT PA6, DRY
Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing..
Die Temperature 215 °C
419 °F
Taiwan PU Corporation TPUI-T64D Transparent Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Die Temperature 215 °C

@Pressure 5.00 - 20.0 MPa
419 °F

@Pressure 725 - 2900 psi
Extrusion
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Die Temperature 215 °C

@Pressure 5.00 - 20.0 MPa
419 °F

@Pressure 725 - 2900 psi
Extrusion
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Die Temperature 215 °C

@Pressure 5.00 - 20.0 MPa
419 °F

@Pressure 725 - 2900 psi
Extrusion
Alliance Polymers Viprene™ G45D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Die Temperature 215 °C
419 °F
Extrusion
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer
Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Die Temperature 215 °C
419 °F
Extrusion
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer
Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Die Temperature 215 °C
419 °F
Extrusion
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer
Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Die Temperature 215 °C

@Pressure 5.00 - 20.0 MPa
419 °F

@Pressure 725 - 2900 psi
Extrusion
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Die Temperature 215 °C

@Pressure 5.00 - 20.0 MPa
419 °F

@Pressure 725 - 2900 psi
Extrusion
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Die Temperature 215 °C
419 °F
Extrusion
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer
Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Copyright © lookpolymers.com All Rights Reserved