Processing Properties Metric English Comments
Feed Temperature 160 - 170 °C
320 - 338 °F
Multibase TPSiV® 4000-80A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
Feed Temperature 160 - 170 °C
320 - 338 °F
Multibase TPSiV® 4200-50A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Feed Temperature 160 - 170 °C
320 - 338 °F
Co-extrusion with Polyamide
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film
The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng..
Feed Temperature 160 - 165 °C
320 - 329 °F
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film
The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut..
Feed Temperature 160 - 170 °C
320 - 338 °F
Co-extrusion with Polyamide
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film
The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength..
Feed Temperature 160 - 175 °C
320 - 347 °F
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film
The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product..
Feed Temperature 160 °C
320 °F
Extrusion
Huntsman IROGRAN® CA116-201 TPU-Polyester
Introduction: IROGRAN CA116-201 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-201 is part of the HUNTSMAN film and shee..
Feed Temperature 160 - 180 °C
320 - 356 °F
Lavergne VYTEEN ABS 2901 Acrylonitrile Butadiene Styrene
Vyteen ABS 2901 is a black recycled general purpose ABS terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Good resilience -Good processabi..
Feed Temperature 160 °C
320 °F
Extrusion Coating
DuPont™ Appeel® 20D828 Ethylene Acrylate
Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp..
Feed Temperature 160 °C
320 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Feed Temperature 160 °C
320 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Feed Temperature 160 °C
320 °F
Extrusion Coating
DuPont™ Bynel® 22E757 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Feed Temperature 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Feed Temperature 160 °C
320 °F
Cast Film/Sheet Processing
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Feed Temperature 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 4140 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE
BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru..
Feed Temperature 160 °C
320 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE
BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru..
Feed Temperature 160 °C
320 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Feed Temperature 160 °C
320 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Feed Temperature 160 °C
320 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Feed Temperature 160 °C
320 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Feed Temperature 160 °C
320 °F
Extrusion Coating
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Feed Temperature 160 °C
320 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..