Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 160 - 170 °C | 320 - 338 °F | |
Multibase TPSiV® 4000-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Feed Temperature | 160 - 170 °C | 320 - 338 °F | |
Multibase TPSiV® 4000-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Feed Temperature | 160 - 170 °C | 320 - 338 °F | Co-extrusion with Polyamide |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Feed Temperature | 160 - 165 °C | 320 - 329 °F | |
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut.. |
|||
Feed Temperature | 160 - 170 °C | 320 - 338 °F | Co-extrusion with Polyamide |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Feed Temperature | 160 °C | 320 °F | Extrusion |
Huntsman IROGRAN® CA116-201 TPU-Polyester Introduction: IROGRAN CA116-201 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-201 is part of the HUNTSMAN film and shee.. |
|||
Feed Temperature | 160 °C | 320 °F | Extrusion Coating |
DuPont™ Appeel® 20D828 Ethylene Acrylate Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Feed Temperature | 160 °C | 320 °F | Blown Film Coextrusion |
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Feed Temperature | 160 °C | 320 °F | Blown Film Coextrusion |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Feed Temperature | 160 °C | 320 °F | Cast Film/Sheet Processing |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 4033 Anhydride Modified HDPE BYNEL® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 4140 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 4140 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | Extrusion Coating |
DuPont™ Appeel® 20D784 Ethylene Acrylate Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature .. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Feed Temperature | 160 °C | 320 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 1706 Zinc Ionomer Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |