DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer DuPont
Trade Name Bynel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylene (PP) resins. Physical properties of BYNEL Series 5000 resins are typical of polypropylene resins with similar density and melt flow rates. BYNEL 5000 series resins adhere to a variety of materials. They are most often used to adhere to PP, EVOH and polyamide. These resins are designed for applications in which EVOH or polyamide is melt coextruded with PP or PP copolymers. BYNEL 50E725 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the use of adhesive interlayers in composite packages for food use. This regulation describes adhesives which may be safely used as components of articles intended for use in packaging, transporting or holding food. This regulation requires that either (1) the adhesive is separated from the food by a functional barrier, or (2) the quantity of adhesive which contacts fatty or aqueous foods does not exceed the trace amounts at the seams or edges. Customers should satisfy themselves that the food contact material is serving as a functional barrier to the adhesive.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792, ISO 1183
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 100 °C
212 °F
Freezing Point; ASTM D3418
144 °C
291 °F
ASTM D3418, ISO 3146
Vicat Softening Point 114 °C
237 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 260 °C
<= 500 °F
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
160 °C
320 °F
CoExtrusion with Nylon Processing
Zone 2 210 °C
410 °F
CoExtrusion with EVOH Processing
210 °C
410 °F
CoExtrusion with Nylon Processing
Zone 3 235 °C
455 °F
CoExtrusion with EVOH Processing
260 °C
500 °F
CoExtrusion with Nylon Processing
Zone 4 235 °C
455 °F
CoExtrusion with EVOH Processing
260 °C
500 °F
CoExtrusion with Nylon Processing
Zone 5 235 °C
455 °F
CoExtrusion with EVOH Processing
260 °C
500 °F
CoExtrusion with Nylon Processing
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
260 °C
500 °F
CoExtrusion with Nylon Processing
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
260 °C
500 °F
CoExtrusion with Nylon Processing
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
<= 260 °C
<= 500 °F
CoExtrusion with Nylon Processing