Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7786 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Emergency running property.Improved wear behaviour, low warpage.High chemical resistance p.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7809/BK PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-8053/EM/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-8160 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-8199 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-8279 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Drying Temperature | 120 °C @Time >=28800 sec |
248 °F @Time >=8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1850/TF/30 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1850-7783-1 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 120 °C @Time 7200 - 14400 sec |
248 °F @Time 2.00 - 4.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Drying Temperature | 120 °C @Time 7200 - 14400 sec |
248 °F @Time 2.00 - 4.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 80-7555 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Drying Temperature | 120 °C @Time 7200 - 14400 sec |
248 °F @Time 2.00 - 4.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 80-7713 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Drying Temperature | 120 °C @Time 7200 - 14400 sec |
248 °F @Time 2.00 - 4.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 80-8268 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Drying Temperature | 120 °C @Time 14400 sec |
248 °F @Time 4.00 hour |
dehumidifying dryer |
LG Chemical Lupox® HV-1010 General Purpose PBT, Unreinforced, High Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105/GF/30/TF/15 PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7709/RD PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Drying Temperature | 120 °C @Time >=28800 sec |
248 °F @Time >=8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1106-8133 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Drying Temperature | 120 °C @Time >=28800 sec |
248 °F @Time >=8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/BK PBT, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7980 PEEK, with carbon fiber Applications: medical engineeringHigh-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flamm.. |
|||
Drying Temperature | 120 °C @Time 14400 sec |
248 °F @Time 4.00 hour |
dehumidifying dryer |
LG Chemical Lupox® GP-2151F General Purpose PBT, 15% Glass Fiber Reinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Drying Temperature | 120 °C @Time 18000 sec |
248 °F @Time 5.00 hour |
Chute Hot-Wind |
Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Electric Cabinet BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 120 °C @Time 14400 sec |
248 °F @Time 4.00 hour |
Chute Hot-Wind |
Zhejiang Juner PC-A1-18 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 120 °C @Time 14400 sec |
248 °F @Time 4.00 hour |
Chute Hot-Wind |
Zhejiang Juner PC-A1-33 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 120 °C @Time >=28800 sec |
248 °F @Time >=8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Drying Temperature | 120 °C @Time 18000 sec |
248 °F @Time 5.00 hour |
|
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |