Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 5.00 - 6.00 min | 5.00 - 6.00 min | |
Northstar Polymers MPP-M09D "Slow Cure" Semi-Rigid Foam Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is set longer than ordinary rigid foam formulatio.. |
|||
Pot Life | 5.00 min | 5.00 min | |
Northstar Polymers MPP-W43C Polyurethane Gel MPP-W43C is a polyurethane gel formulation specifically designed for padding and cushioning applications that require Shore Durometer OOO scale hardness materials. With this material, a user can ob.. |
|||
Pot Life | 5.00 min @Temperature 23.9 °C |
5.00 min @Temperature 75.0 °F |
|
ITW Devcon Plastic Steel® Metal Repair 5 Minute® Putty (SF), Dark Grey Information provided by ITW Devcon |
|||
Pot Life | 5.00 min @Temperature 25.0 °C |
5.00 min @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6126 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Pot Life | 5.00 min | 5.00 min | Open Time |
Valley Adhesives EM-105 High Performance Application Glue Stick Valley Adhesives EM-105 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol.. |
|||
Pot Life | 5.00 min | 5.00 min | Open Time |
Valley Adhesives EM-110 High Performance Application Glue Stick Valley Adhesives EM-110 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol.. |
|||
Pot Life | 5.00 min | 5.00 min | Open Time |
Valley Adhesives EM-120 High Performance Application Glue Stick Valley Adhesives EM-120 High Performance Application Glue StickGeneral purpose hot melt spray adhesive; High performance and heat resistance with excellent adhesion, shear, peel and high initial str.. |
|||
Pot Life | 5.00 min @Temperature 25.0 °C |
5.00 min @Temperature 77.0 °F |
|
Tra-Con Tra-Bond 216R02 Quick Set Electrical Insulator TRA-BOND 216R02 is an exceptional epoxy formulation recommended for applications where both quick set-up and a low-viscosity material are required. This clear, two-part, low-viscosity system is easi.. |
|||
Pot Life | <= 5.00 min @Temperature 25.0 °C |
<= 5.00 min @Temperature 77.0 °F |
100 g |
Armstrong A-10-T Epoxy Adhesive Clear, thixotropic, 5-minute cure general-purpose epoxy adhesive. Provides rapid high strength bonds to many substrates. Supplied in 1:1 ratio dispense kits for easy application.Information provid.. |
|||
Pot Life | <= 5.00 min @Temperature 25.0 °C |
<= 5.00 min @Temperature 77.0 °F |
100 g |
Armstrong A-7 Epoxy Adhesive Clear, flexible, 5-minute cure structural bonding plastic adhesive. Develops high performance, high impact durable bonds for operating temperatures from -65° to +250°. Supplied in 1:1 ratio dispe.. |
|||
Pot Life | 5.00 min | 5.00 min | uncured |
Atom Adhesives AA-BOND 2156 Epoxy Adhesive AA-BOND 2156 is a thixotropic (smooth paste) thermally conductive epoxy system. It is used for staking heat sinks, transistors, diodes, resistor, integrated circuits and other heat-sensitive compone.. |
|||
Pot Life | 5.00 min | 5.00 min | uncured |
Atom Adhesives AA-BOND F125 Epoxy Adhesive AA-BOND F125 is a 8 minutes gelling epoxy recommended for use in fiber optic connectors, optical and industrial bonding applications. AA-BOND F125 is clear, two part system is easily mixed and used .. |
|||
Pot Life | 5.00 min @Temperature 23.9 °C |
5.00 min @Temperature 75.0 °F |
|
Devcon Zip Patch™ Epoxy Emergency Repair ProductsComments: High-technology, adhesive-impregnated, putty patching system that cures at room temperature. Hardens to a tough, durable, waterproof finish in minutes. Easy-to-u.. |