Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 9.00 - 180 min | 9.00 - 180 min | Average value: 64.2 min Grade Count:28 |
Overview of materials for Epoxy Adhesive, Flexible This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro.. |
|||
Pot Life | 120 - 180 min @Temperature 20.0 °C |
120 - 180 min @Temperature 68.0 °F |
|
Permabond ET538 Epoxy Resin PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia.. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 gm mass |
Resin Technology Group TIGA 159 LV-UV Low Viscosity, Quick Gel UV Initiated, Flexible Epoxy Adhesive Mix ratio 2 to 1 by volume.TIGA 159 LV-UV hybrid epoxy system is a low viscosity adhesive designed for small potting applications, bonding, laminating, sealing and structural repair applications whe.. |
|||
Pot Life | 120 - 180 min | 120 - 180 min | Ready for topcoating |
Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul.. |
|||
Pot Life | 120 - 180 min @Temperature 23.9 °C |
120 - 180 min @Temperature 75.0 °F |
|
Devcon Tile Adhesive Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Pot Life | 120 - 180 min | 120 - 180 min | |
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr.. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 g |
Armstrong A-4/E Epoxy Adhesive Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe.. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 g |
Armstrong A-5/E Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 g |
Armstrong C-1/E Epoxy Adhesive A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor.. |
|||
Pot Life | 120 - 180 min @Temperature 24.0 °C |
120 - 180 min @Temperature 75.2 °F |
|
BCC Products BC 7020 Epoxy Backfill System BC 7020 is a lightweight two component epoxy backfill system. Unlike BC 7010, the filler portion is pre-blended into the resin and hardener components for easier handling, thus simplifying the mixin.. |
|||
Pot Life | 120 - 180 min | 120 - 180 min | |
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina Coarse grain castable for producing large hi-temp tooling. |
|||
Pot Life | 120 - 180 min | 120 - 180 min | |
Abatron AboCast 22-30/AboCure 50-4 Epoxy AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 g |
Armstrong A-1/E Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 g |
Armstrong A-3/E Epoxy Adhesive A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,.. |
|||
Pot Life | 120 - 180 min | 120 - 180 min | |
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils .. |
|||
Pot Life | 120 - 180 min | 120 - 180 min | |
Abatron AboCast 50-11/AboCure 50-4 Epoxy AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
1-2 lbs |
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge cas.. |