Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 22-30/AboCure 50-4 Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 22-30/AboCure 50-4 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. AboCast 22-30/AboCure 50-4 is a slow, thick, filled, black, opaque, room-temperature-cure, medium-viscosity epoxy system. It is the preferred system for most casting applications. It offers good thermal conductivity, minimum shrinkage, and low exotherm (heat of reaction). AboCure 50-4 can be mixed in ratios variable from 16 to 50 pbw with 100 pbw AboCast 22-30 for different cured properties: higher rigidity, chemical and heat resistance with the lower AboCure ratios (16-20 pbw), or higher flexibility with higher ratios. The converter offers the lower exotherm that permits unusually heat-sensitive or large castings. The system is used for encapsulation, potting, and assembly of electronic and magnetic components, such as: capacitors, transformers, terminals, industrial magnets, small and large magnetic assemblies, metal detectors, metal separators, magnetic printing cylinders, magnetic holders, insulators, junction boxes, switches, and circuit boards. It is also used in general-purpose casting and bonding for structural and dielectric applications.
Physical Properties Metric English Comments
Density 0.959 g/cc
0.0346 lb/in³
AboCure 50-4
1.49 g/cc
0.0537 lb/in³
AboCast 22-30
Water Absorption 0.19 %

@Time 605000 sec
0.19 %

@Time 168 hour
Viscosity 18600 cP
18600 cP
Mechanical Properties Metric English Comments
Compressive Strength 92.4 MPa
13400 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 8.10e+15 ohm-cm
8.10e+15 ohm-cm
"A"
Processing Properties Metric English Comments
Pot Life 120 - 180 min
120 - 180 min
Descriptive Properties Value Comments
Color Black
Parts by Weight (pbw) 100
AboCast 22-30
25
AboCure 50-4
Copyright © lookpolymers.com All Rights Reserved