Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 120 min | 120 min | |
Resin Technology Group 1217 Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | 120 min | 120 min | |
Resin Technology Group DPE110698-1 Two component Potting Compound Resin Technology Group DPE110698-1 Two component Potting CompoundClear, fire retardant, low viscosity potting compound. |
|||
Pot Life | >= 120 min | >= 120 min | Mass: 50g |
Resinlab® EP691 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP 691 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting.. |
|||
Pot Life | >= 120 min | >= 120 min | |
Abatron 7505-2A/501B Filled Potting Compound
(discontinued **) Black and colors filled viscous epoxy system to seal heat probes. 100/20 variable ratio.Information provided by Abatron. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
4 fl. Oz.; ASTM D2471 |
Fibre Glast Saf-T-Poxy 2410 / 2184 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |
|||
Pot Life | >= 120 min | >= 120 min | |
ACC QSil 551 QSI Quantum Silicones Silicone Potting Material
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: 100% solid, long pot life, low modulus, good elongation. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
4 fl. Oz.; ASTM D2471 |
Fibre Glast 2000 / 2120 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
Pot Life | 120 min | 120 min | |
Lord Adhesives 3170 Two-component, high cold strength, cryogenic application Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 120 min | 120 min | |
Lord Adhesives Aeroglaze® M1433 Elastomeric Polyurethane Rain Erosion Coating Aeroglaze® M1433 elastomeric coating functions exceptionally well in abrasive environments. Inherent flexibility, corrosion resistance, and energy absorptive properties make Aeroglaze M1433 elast.. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
50% relative humidity |
Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane Chemglaze® M331 is a two package, ASTM D-16 Type IV elastomeric polyurethane coating. Cured films produced from this coating are tough, flexible, and resistant to erosion, abrasion, and impact. T.. |
|||
Pot Life | 120 - 150 min | 120 - 150 min | 100 gram mass |
Master Bond EP21SC-1 Two Component Epoxy Resin System Product Description: Master Bond Polymer System EP21SC-1 is a two component epoxy system featuring abrasion resistance. This high performance compound utilizes silicon carbide as a filler material a.. |
|||
Pot Life | 120 min | 120 min | 25 grams |
Tra-Con Tra-Bond F123MV Color Keyed High Temperature Epoxy Adhesive TRA-BOND F123 MV is a fast cure, medium viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminati.. |
|||
Pot Life | 120 min | 120 min | |
Tra-Con Tra-Cast F311 Optically Transparent Semi-Flexible Casting System TRA-CAST F311 is a clear, low viscosity epoxy formulation developed for molding, embedding, casting and potting applications where clarity, toughness, long pot-life and superior impact properties ar.. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
100 grams |
Trelleborg Emerson & Cuming Eccobond® 15 LV Clear Variable Hardness Low Viscosity Catalyst Emerson & Cuming 15 LV Clear Eccobond® Variable Hardness Low Viscosity CatalystLow viscosity. Easy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener .. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
100 grams |
Trelleborg Emerson & Cuming Eccobond® 15 LV Variable Hardness Low Viscosity Catalyst Emerson & Cuming 15 LV Eccobond® Variable Hardness Low Viscosity CatalystLow viscosity. Easy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener used. .. |
|||
Pot Life | 120 min | 120 min | |
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a .. |
|||
Pot Life | 120 min | 120 min | |
Loctite® Durabond® E-120HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 120 min @Temperature 23.9 °C |
120 min @Temperature 75.0 °F |
|
Devcon Wear Guard (High Temp) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Pot Life | 120 min | 120 min | |
Epoxy Technology EPO-TEK® T7109-19 Electrically Insulating Epoxy Paste Material Description: A flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications. It is an alternative to EPO-TEK® T7109-17, de.. |
|||
Pot Life | 120 min | 120 min | |
Epoxyset Epoxibond EB-348 Low Expansion Epoxy Adhesive EB-348 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional .. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
200 g |
Abatron AboCast/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 g |
Armstrong A-4/E Epoxy Adhesive Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe.. |
|||
Pot Life | 120 min | 120 min | |
Abatron 8509-4 A/B Carbon-Filled Electrically Conductive Epoxy Compound 8509-4 A/B is a solventless carbon-epoxy system used as an adhesive and silk-screening material with anti-static and other lower-conductivity requirements. |
|||
Pot Life | 120 min | 120 min | 100 g |
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 g |
Armstrong A-3/E Epoxy Adhesive A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,.. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
100 gm mass |
Aremco Aremco-Bond™ 2315 High Performance Epoxide High Temperature, Low Viscosity, Potting Compound for Electrical Applications. |
|||
Pot Life | >= 120 min | >= 120 min | |
Abatron 8311-8A/82033B Filled Potting Compound
(discontinued **) Gray and colors casting, potting, embedding, and adhesive epoxy system. 40% filled. 100/8 ratio.Information provided by Abatron. |
|||
Pot Life | 120 min @Temperature 80.0 °C |
120 min @Temperature 176 °F |
|
Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy Clear amber, high viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components t.. |