Polymer Property : Injection Pressure = 50.0 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Average value: 45.0 MPa Grade Count:5
Overview of materials for Nylon 12, Extrusion/Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values ..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3020GX9 23% Glass Fiber Reinforced Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: 23% glass fiber reinforced gradeInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3020X15 Nylon 12 Thermister
Description: UBESTA Nylon 12 ThermisterInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3020X25L Rigid Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: for coating steel and aluminumInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3020X8 Nylon 12 Thermister
Description: UBESTA Nylon 12 ThermisterInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JI9L 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability, designed for high burst pressure performance at high temperat..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JLX2 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability Information provided by UBE.
Injection Pressure 2.00 - 50.0 MPa
290 - 7250 psi
Melt Pressure
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Toyobo GLAMIDE® T-714E Transparent Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12
Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12
Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE.
Injection Pressure 2.00 - 50.0 MPa
290 - 7250 psi
Melt Pressure
Wacker Silicones Geniomer® 80 Silicone TPE
SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Injection Pressure 2.00 - 50.0 MPa
290 - 7250 psi
Melt Pressure
Wacker Silicones Geniomer® 60 Silicone TPE
SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..