Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 50.0 - 80.0 MPa | 7250 - 11600 psi | |
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Injection Pressure | 50.0 - 70.0 MPa | 7250 - 10200 psi | |
Polykemi AB POLYfill PP CQX15015 R3 UV Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Injection Pressure | 50.0 - 150 MPa | 7250 - 21800 psi | |
Solvay Specialty Polymers Primef® 7010 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less flu.. |
|||
Injection Pressure | 50.0 - 103 MPa | 7250 - 15000 psi | Average value: 82.5 MPa Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Injection Pressure | 50.0 - 120 MPa | 7250 - 17400 psi | |
Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Injection Pressure | 50.0 - 120 MPa | 7250 - 17400 psi | |
Gromax PBT 2000-104D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Injection Pressure | 50.0 - 110 MPa | 7250 - 16000 psi | Specific |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Injection Pressure | 50.0 - 110 MPa | 7250 - 16000 psi | |
Zhejiang Juner PA66-301-G20 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Framework of CoilsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 50.0 - 60.0 MPa | 7250 - 8700 psi | |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 50.0 - 120 MPa | 7250 - 17400 psi | |
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |