Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | <= 285 °C | <= 545 °F | |
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr.. |
|||
Processing Temperature | <= 285 °C | <= 545 °F | |
DuPont™ HPF® 1000 Amorphous Polymer for Golf Balls DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a hig.. |
|||
Processing Temperature | <= 285 °C | <= 545 °F | |
DuPont™ HPF® 2000 Amorphous Polymer for Golf Balls DuPont™ HPF 2000 offers high COR and lower compression. This combination of properties makes it extremely versatile and possible for this polymer to be used as a core, mantle, or cover in a golf ba.. |
|||
Processing Temperature | <= 285 °C | <= 545 °F | |
DuPont™ Surlyn® 8528 Sodium Ionomer Surlyn® 8528 is a sodium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 8528 thermoplastic resi.. |
|||
Processing Temperature | <= 285 °C | <= 545 °F | |
DuPont™ Surlyn® 9320 Zinc Ionomer Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin .. |
|||
Processing Temperature | <= 285 °C | <= 545 °F | |
DuPont™ Surlyn® 6320 Magnesium Ionomer Surlyn® 6320 is a magnesium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 6320 thermoplastic r.. |
|||
Processing Temperature | 285 - 300 °C | 545 - 572 °F | Melt |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Processing Temperature | 285 - 305 °C | 545 - 581 °F | Melt |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Processing Temperature | 285 - 305 °C | 545 - 581 °F | Melt |
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free.. |
|||
Processing Temperature | 285 - 305 °C | 545 - 581 °F | |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Processing Temperature | <= 285 °C | <= 545 °F | |
DuPont™ Surlyn® 1706 Zinc Ionomer Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Processing Temperature | <= 285 °C | <= 545 °F | |
DuPont™ Surlyn® 1707 Sodium Ionomer Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Processing Temperature | <= 285 °C | <= 545 °F | |
DuPont™ Surlyn® 1825 Zinc Ionomer Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp.. |
|||
Processing Temperature | <= 285 °C | <= 545 °F | |
DuPont™ Surlyn® 2601B Sodium Ionomer Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer .. |
|||
Processing Temperature | 285 - 300 °C | 545 - 572 °F | Melt |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Processing Temperature | 285 - 305 °C | 545 - 581 °F | Melt |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Processing Temperature | 285 - 305 °C | 545 - 581 °F | Melt |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Processing Temperature | 285 - 305 °C | 545 - 581 °F | Melt |
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Processing Temperature | 285 - 305 °C | 545 - 581 °F | Melt |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |