Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 177 - 188 °C | 350 - 370 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-1038 Natural 85 PVC Compound Application: A 60 - 75°C general purpose, sunlight resistant compound suitable for jacketing applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 177 - 182 °C | 350 - 360 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-7056-1002 PVC Compound Application: A 75°C Jacketing Compound UL approved for 720 hr. sunlight resistance. Suitable for use in direct burial applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 177 - 230 °C | 350 - 446 °F | Average value: 199 °C Grade Count:29 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Processing Temperature | 177 - 230 °C | 350 - 446 °F | Average value: 199 °C Grade Count:8 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Processing Temperature | 177 - 216 °C | 350 - 420 °F | Extrusion |
Shuman 710H Utility Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 177 - 216 °C | 350 - 420 °F | Extrusion |
Shuman 730 Utility White ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the Shuman Plastics, Inc. |
|||
Processing Temperature | 177 - 216 °C | 350 - 420 °F | Extrusion |
Shuman 780H Grey ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 177 - 191 °C | 350 - 375 °F | Recommended Stock Temperature |
Sylvin Technologies 5748 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 177 °C @Time 3600 - 7200 sec |
350 °F @Time 1.00 - 2.00 hour |
|
Master Bond FLM36 B-staged film for high performance bonding and sealing Master Bond FLM36 is a film adhesive with exceptional strength properties, high temperature resistance and first class thermal conductivity and electrical insulation properties. Based on the Master .. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo Gem-Tone GC-13P Ruby Red Gem-Tone® GC-13P Ruby Red is a rich, strong blue shade red colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo Gem-Tone GC-18F Emerald Green Gem-Tone® GC-18F Emerald Green is a rich, strong green colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of .. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-11 Aurora Pink DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-12 Neon Red DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-15 Blaze Orange DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-16 Arc Yellow DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-19 Horizon Blue DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | >= 177 °C | >= 350 °F | |
DayGlo ZQ Pigments ZQ-21 Corona Magenta DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 2060 CL Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 2080 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 2090 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 3075 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys DURACRYN 8070 NC Thermoplastic Rubber Information provided by Advanced Polymer Alloys |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 2080 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 °C | 350 °F | |
Advanced Polymer Alloys Alcryn® 2090 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Processing Temperature | 177 - 230 °C | 350 - 446 °F | Average value: 198 °C Grade Count:17 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Processing Temperature | 177 - 230 °C | 350 - 446 °F | Average value: 199 °C Grade Count:24 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Processing Temperature | 177 - 188 °C | 350 - 370 °F | Recommended Stock Temperature |
Sylvin Technologies 6055 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |