Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
Kleerdex Kydex® 130 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Decorative thermoplastic sheetApplications: Appliances, laminations, electronics, in-store displays, medical devices, equipment housings, dental equipmentFeatures: For deep to hard to form parts or .. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
Kleerdex Kydex® L Acrylic/PVC Thermoplastic Sheet
(discontinued **) Laminating grade fire rated sheetApplications: Store fixtures and displays, exhibits, service counters, doors, partitionsFeatures: Toughness and durability, solid, integral color, chemical resistanc.. |
|||
Processing Temperature | 163 °C | 325 °F | Cure Schedule: 20 min @ 163°C |
Huntsman HT 9690 Special Hardener Mix Ratio with ECN 1299 is 50.Comments/Applications: 0-cresol novolac hardener. *Mix ratio with ECN 1299. Latent with ECN resins. High temperature resistant. Molding compound and powder coatin.. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 399 °F | Thermoforming |
KYDEX® 430 ABS/PVC Blend for Medical Device Housings KYDEX® 430 is an ABS/PVC thermoplastic sheet that offers superior thermoformability, rigidity, breakage resistance, chemical resistance and fire retardancy.Features:Good for deep or hard to form .. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming |
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp.. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
KYDEX® T Acrylic/PVC Thermoplastic Sheet Impact resistant fire rated sheetApplications: External housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for equipment such as v.. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
KYDEX® 6185 Thermoplastic Sheet High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar.. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest sh.. |
|||
Processing Temperature | 163 - 174 °C | 325 - 345 °F | Recommended Stock Temperature |
Sylvin Technologies 5132-75 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-026 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-028 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-050 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-051 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-072 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-082 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-089 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-116 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-214 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 168 °C | 325 - 335 °F | |
Axiall 3014 Rigid PVC, Extrusion Georgia Gulf 3014 is a base for use of wood flour up to 40 percent. Impact Strength & ToughnessFlame RetardantChemical ResistanceDimensional StabilityInformation provided by Georgia GulfGeorgia Gul.. |
|||
Processing Temperature | 163 - 168 °C | 325 - 335 °F | |
Axiall 3020 Rigid PVC, Extrusion Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-251 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
Kleerdex Kydex® 200 Acrylic/PVC Thermoplastic Sheet
(discontinued **) General purpose gradeApplications: Can be used to substitute effectively for both general purpose ABS and acrylic/PVC thermoplastics. Examples include data processing equipment housings, photocopy .. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
Kleerdex Kydex® 510 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable and decorative sheetApplications: Housings for equipment, recreation vehicles and truck parts, safety equipment, building products, signage, wall panels, facia, doors, service counters, .. |
|||
Processing Temperature | 163 - 174 °C | 325 - 345 °F | Recommended Stock Temperature |
Sylvin Technologies 5123 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |