Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 188 - 227 °C | 370 - 440 °F | Average value: 204 °C Grade Count:3 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:8 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:3 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:7 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:7 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Processing Temperature | 40.0 - 227 °C | 104 - 440 °F | Average value: 183 °C Grade Count:23 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 710 Utility Black ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 710H Utility Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 720 Black ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 720H Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 730 Utility White ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 730H White ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 780 Grey ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 780H Grey ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 790 Black and Custom Colors ABS-Flame Retardant Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 791 Black and Custom Colors ABS-Flame Retardant Long term thermal aging rated. Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 810 Black Polystyrene High Impact Good impact strength, injection molding and extrusion grades, easy processability, good surface appearance, good gloss.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 811 Black Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 880 Grey Polystyrene High Impact Good impact strength, injection molding and extrusion grades, easy processability, good surface appearance, good gloss.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 881 Grey Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | |
Shuman SP810 Black Polystyrene High Impact Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | |
Shuman SP880 Grey Polystyrene High Impact Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 188 - 227 °C | 370 - 440 °F | Blow Molding Stock Temp. |
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 211 °C Grade Count:15 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:5 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Processing Temperature | 188 - 227 °C | 370 - 440 °F | Average value: 209 °C Grade Count:8 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:4 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |