Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 190 - 210 °C | 374 - 410 °F | Cylinder temp |
Asahi Kasei Tenac® 2013A Acetal Homopolymer, UV Stabilized
(discontinued **) Similar to 3013A, but higher in molecular weight.Applications: Pipe fittings, rollers, exterior automotive parts.This product is not a part of the standard product line dated 2003. |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | Cylinder temp |
Asahi Kasei Tenac® LT805 Acetal Homopolymer, Low Friction Grade
(discontinued **) Excellent friction and wear on metals.Applications: Keyboard parts, bearings for office machines, gears.This product is not a part of the standard product line dated 2003. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
Taiwan Sheen Soon Sheenthane® A9315E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 190 - 210 °C | 374 - 410 °F | |
Wanhua Chemical Wanthane® WHT-2190 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | Extrusion Temp |
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 422351S SBS Based Material, 35D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 500400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 500500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 500650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 600800S SEBS Based Material, Filled Qualities, 80A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 660900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 662800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Processing Temperature | 194 - 210 °C | 381 - 410 °F | Optimum Extrusion Conditions |
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 600400S SEBS Based Material, Filled Qualities, 40A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 300 HI2 POM Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Processing Temperature | 180 - 210 °C | 356 - 410 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 300 HI4 POM High impact strength grade, high damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Processing Temperature | 205 - 210 °C | 401 - 410 °F | Injection |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |