Wanhua Chemical Wanthane® WHT-2190 Polycaprolactone Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-2190 Polycaprolactone Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength 29.0 MPa
4210 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
300% Modulus 0.0140 GPa
2.03 ksi
ASTM D412
Tear Strength 120 kN/m
685 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F